Excellent resistance to ferric and cupric chlorides, mineral acids, chlorinated environments, formic and acetic acids, sea water and brine. Resistant to oxidation at temperatures up to 1040ºC (1900°F). It is widely used in chemical, petrochemical and oil industries.
- ABTN | ASTM | SAE | AISI: Alloy C-4 | ASTM B574 | UNS N06455
- DIN | WNr: DIN 17744 | WNr 2.4610
- Chemical composition:
C % | Si % | Mn % | Cr % | Ni % | Fe % | Ti % | OTHERS % |
max. 0.015 | max. 0.08 | max. 1.0 | 14.0 – 18.0 | rest | max. 3.0 | max 0.7 | Mo=14.0 – 17.0 | Co=max. 2.0 P=max. 0.025 | S=max. 0.015 |